UNS S42200 chemical composition
C 0.20-0.25
Si ≤0.50
Mn 0.50-1.00
P≤0.030
S≤0.025
Ni 0.50-1.00
Cr 11.0- 12.50
Mo 0.90-1.25
W 0.90-1.25
V 0.20-0.30
Cu≤0.30
UNS S42200 Mechanical properties
Tensil strength 930MPa min
yield strength 760MPa min
Elongation 12 % min
Reduction of area 32% min
Charpy Akv 11J
hardness :280-341 HBW
Note: the datasheet is just for reference
UNS S42200 Delivery Condition:
Hot-rolled / hot forged
black surface/ peeled surface / rough turned surface
annealed / heat treatment
fixed length / random length
UNS S42200 is used in applications such as compressors or steam turbines and also in aircraft parts, valves, high temperature bolting etc.